Next crossmember reinforcement is welded in.
Typical repair sequence: Corner of shelf that forms base of rear seat is nasty. First step is to define area to replace.
Next, before any old metal is cut, a patch is fabricated and test fitted.
Now the garbage can be cut out. Cut-off wheel and nibbler are the heavy artillery, cold chisel and ball peen hammer are the basic infantry weapons.
The affected area is trimmed, blasted, ground, chemically treated and primed with Weld-Thru.
Patch is welded in place with many small tacks.

Continued... p8 p9 p10 p11 p12 p13 p14

back to part 1

Questions? Comments?

Copyright © 2001 AlfaCentro & Forza Modern Media. All rights reserved. Neither AlfaCentro.com, it's publisher, FORZA Modern Media, LLC., or the individual article authors makes any warranties, expressed or implied, that the techniques, modifications, and procedures outlined in these stories are free of errors and omissions, meet applicable safety standards, or are suitable for the purposes described. The publisher and authors also expressly disclaim all liability for damages that may arise from the use of information presented in these articles.